Dow Engage® Polyolefin Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. Engage® features extended part/product life over Styrene Block Copolymers; improved flexibility and crck-resistance vs. EVA or EMA; improved processibilty and enhanced properties vs. flexible PVCs; and greater durability vs. EPDM or EPR. Property data below shows the range of typical properties. Information provided by DuPont Dow Elastomers.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- Flexural Modulus
- Melting Point
- Brittleness Temperature
- Haze
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|