Dow Engage® 8150 Polyolefin Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Description: Engage® 8150 and Engage® 8157 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and provide superb impact properties in blends with polypropylene (PP) and polyethylene (PE). They are widely used in TPO applications where excellent low temperature impact properties are desired. Engage® 8150 and Engage® 8157 also provide high filler loading capability and outstanding peroxide cure capability. When crosslinked by peroxide, silane, or irradiation, they give exceptional heat aging, compression set, and weather resistance properties, and may be used to produce high performance electrical insulation. Engage® 8157 is Engage® 8150 with a nominal loose talc coating. The talc is untreated, with a 1 micron particle size. The product form is free-flowing pellets. Information provided by manufacturer.
| Available Properties |
- Density
- Mooney Viscosity
- Melt Index of Compound
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- 2% Secant Modulus
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
- Comonomer Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|