Dow Engage® 8411 Polyolefin Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Description: Engage® 8411 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable injection molded industrial and consumer goods and compression molded gaskets. Engage® 8411 provides high clarity in products requiring visual inspection and allows the use of hot runner molds to enhance production efficiency. In addition, its low density can help control resin and production costs, while reducing the weight of end products. Engage® 8411 also provides good impact properties in blends with polypropylene (PP) and polyethylene (PE), especially in applications like automotive thermoplastic olefins (TPOs), requiring high melt flow modifiers. Information provided by manufacturer.
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- 2% Secant Modulus
- Melting Point
- Vicat Softening Point
- Comonomer Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|