Dow Engage® 8842 Polyolefin Elastomer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Description: Engage® 8842 polyolefin elastomer is an ultra-low density ethylene-octene copolymer with a nominal loose talc surface coating. The talc is untreated and has a nominal 1 µm particle size. This product offers the exceptional properties of an ultra-low density elastomer with the added potential of handling this polymer in pellet form. Engage® 8842 has excellent flow characteristics and provides superb impact properties in blends with polypropylene (PP) and polyethylene (PE). It performs well in TPO applications where superior low temperature impact properties are desired. Talc addition significantly improves ability to handle the polymer, but severe blocking can occur if the material is stored under severe conditions (i.e., long duration, elevated temperatures, and/or high weight loadings). To minimize temperature effects, product should be stored at temperatures well below its melting point of 33°C, most preferably below 29°C. Information provided by manufacturer.
| Available Properties |
- Density
- Mooney Viscosity
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- 2% Secant Modulus
- Melting Point
- Brittleness Temperature
- Comonomer Content
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|