Dow Engage® ENR 7447.00 Ethylene-Butene Copolymer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Description: ENR 7447.00 is a high flow, low density ethylene-butene copolymer designed for use in combination with our other elastomers to provide tailored solutions in polymer modification applications. The polymer is available as surface modified pellets for ease in handling and mixing. Information provided by manufacturer.
| Available Properties |
- Density
- Viscosity
- Melt Index of Compound
- Crystallinity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 1% Secant Modulus
- Melting Point
- Crystallization Temperature
- Glass Temperature
- Molecular Weight Distribution
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|