Dow Engage® ENR 8556.00 Ethylene-Octene Copolymer
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Description: ENR 8556.00 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in extrusion applications such as tubing and profiles. This elastomer provides excellent clarity and flexibility for low modulus applications. Its low specific gravity (density) delivers lighter weight parts. The product form is free-flowing pellets. Information provided by manufacturer.
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 2% Secant Modulus
|
|
|
|
| Property Data |