Dow Nordel® IP 3745P EPDM Hydrocarbon Rubber
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Description: This semicrystalline, very low diene containing ethylene-propylene terpolymer (EPDM) has a narrow molecular weight distribution for excellent processing characteristics when used as a neat polymer. It has been designed for property modification of thermoplastics such as polyethylene and polypropylene and can be used in peroxide cured rubber compounds. Information provided by manufacturer.
| Available Properties |
- Density
- Volatiles
- Mooney Viscosity
- Ash
- ENB
- Ethylene
- Molecular Weight Distribution
- Product Form
- Propylene
- Residual Transition Metal
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|