Dow Nordel® IP 4520 EPDM Hydrocarbon Rubber
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Description: Nordel® IP 4520 is an amorphous EPDM grade designed for molded applications. It is ideally suited for injection and transfer molded brake parts, corner moldings, general purpose gaskets and moldings. The combination of low viscosity and low crystallinity allows for good processability, low temperature properties and performance without the addition of a plasticizer. Information provided by manufacturer.
| Available Properties |
- Density
- Volatiles
- Mooney Viscosity
- Ash
- ENB
- Ethylene
- Molecular Weight Distribution
- Product Form
- Propylene
- Residual Transition Metal
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|