Dow Nordel® IP 4570 EPDM Hydrocarbon Rubber
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes: Description: Nordel® IP 4570 is an amorphous EPDM grade designed for extruded applications. It is ideally suited for dense extruded profiles, coolant hose and general purpose moldings. The combination of high viscosity and low crystallinity allows for good balance of processability, extensibility, low-temperature properties and performance. Information provided by manufacturer.
| Available Properties |
- Density
- Volatiles
- Mooney Viscosity
- Ash
- ENB
- Ethylene
- Molecular Weight Distribution
- Product Form
- Propylene
- Residual Transition Metal
|
|
|
|
| Property Data |