Dow Nordel® IP 4570 Dense Extruded Profile
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Key Words: 0625A19-01
Material Notes:
Formulation| Nordel® IP 4570 | 100 | | Zinc Oxide | 5 | | Stearic Acid | 1 | | Sterling ST6630 Black | 175 | | Calcium Oxide | 8 | | Paraffinic Oil | 100 | | Sulfur | 1 | | ZnDBC | 1 | | MBTS | 1.5 | | DPTT | 0.75 | | TMTD | 0.75 | Description: Nordel® IP 4570 is an amorphous EPDM grade designed for extruded applications. It is ideally suited for dense extruded profiles, coolant hose and general purpose moldings. The combination of high viscosity and low crystallinity allows for good balance of processability, extensibility, low-temperature properties and performance. Information provided by manufacturer.
| Available Properties |
- Density
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Compression Set, Elevated Temperature
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|