Dow Nordel® IP 4725P High Hardness Extruded Profile
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Key Words: 001166A06-4
Material Notes:
Formulation| Nordel® IP 4725P | 100 | | N-550 Black | 70 | | Liquid BR (Ricon 153) | 12 | | Ground Calcium Carbonate | 60 | | Precipitated Calcium Carbonate | 60 | | Paraffinic Oil | 15 | | ZnDBC | 0.5 | | TBBS | 1.5 | | TMTD | 0.5 | | DPTH | 0.5 | | Stearic Acid | 1 | | Zinc Oxide | 5 | | Sulfur | 6 | | Vulkalent E/C | 1 | Description: Nordel® IP 4725P is a low viscosity semicrystalline grade which offers ease of processing, fast cure rates and high states of cure with standard sulfur cure systems. It is designed for molded and extruded applications requiring low viscosity, high green strength and high finished hardness. It is ideally suited for high hardness extruded profiles and molded goods. It can also be peroxide cured. Information provided by manufacturer.
| Available Properties |
- Density
- Mooney Viscosity
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 200% Modulus
- Compression Set, Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|