Dow Nordel® IP 4760P Compound
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Material Notes:
Formulation| Nordel® IP 4760P | 100 | | N-550 Black | 80 | | Paraffinic Oil | 50 | | Zinc Oxide | 5 | | Stearic Acid | 1 | | ZnDBC 80% | 2.5 | | TMTD 80% | 0.63 | | MBT | 1.25 | | Sulfur | 1.5 | Description: Nordel® IP 4760P is a semicrystalline, ethylenepropylene-diene (EPDM) terpolymer. The polymer's unique bimodal ethylene distribution provides a balance of processing characteristics not seen in other semicrystalline EPDMs. Nordel® IP 4760P provides better low temperature performance and higher green strength compared to a competitive control polymer. Information provided by manufacturer.
| Available Properties |
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Modulus of Elasticity
- 50% Modulus
- 100% Modulus
- 200% Modulus
- Tear Strength
- Compression Set, Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|