Dow Nordel® IP 4770P Highly Extended Low-Cost Hose
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Key Words: 0639A04-06
Material Notes:
Formulation| Nordel® IP 4770P | 100 | | Zinc Oxide | 5 | | Stearic Acid | 2 | | N-550 Black | 50 | | N-650 Black | 200 | | Ground Calcium Carbonate | 200 | | Parrafin Wax | 2 | | Paraffinic Oil | 75 | | Naphthenic Oil | 125 | | Sulfur | 1 | | MBTS | 1.5 | | ZnDBC | 2 | | ZnDMC | 1 | | TMTD | 1 | | DTDM | 1 | Description: Nordel® IP 4770P is a high molecular weight semicrystalline grade and offers fast cure rates and high states of cure with standard sulfur cure systems. It offers high green strength and high extensibility. It is designed for extruded applications such as profiles and hose. It is also suitable for molded goods. This grade is available in rod form for improved mixing speed and throughput. Information provided by manufacturer.
| Available Properties |
- Density
- Mooney Viscosity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
- 200% Modulus
- 300% Modulus
- Tear Strength
- Compression Set, Elevated Temperature
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|