DuPont Elastomers Hypalon® CP-826 Adhesion Primer, General Description
Subcategory: Elastomer, TS; Thermoset
Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Material Notes: Description: Hypalon CP 826 is a chlorinated, maleic anhydride grafted polypropylene resin. Suggested End Uses: Adhesion primer for: - Polypropylene
- Polypropylene blends with TPOs (auto bumpers)
- Polyurethane foam, (athletic shoe construction)
- EVA with high levels of PE (athletic shoes)
Main Features: Hypalon CP 826 has been developed to have excellent adhesion to polypropylene and blends containing polypropylene. It can be used in dilute solutions as a wash primer or tie layer between materials that are difficult to adhere. It can also be used as an adhesion modifier for coatings, adhesives and inks because of its solubility in commonly used solvents. Hypalon CP 826 is offered in solid form. Information provided by manufacturer.
| Available Properties |
- Density
- Viscosity
- Glass Temperature
- Gardner Color Number
- Chlorine Content
- Product Form
- Saponification Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|