Dow AIM® 4810 High Impact Styrenic Resin
Subcategory: Polystyrene; Thermoplastic
Key Words: HIPS
Material Notes: AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatures than ABS, which may allow faster cycle times, energy savings or an opportunity to fill more complex molds. When used unmodified for the manufacture of food contact articles AIM 4810 complies with the US Food, Drug and Cosmetic Act and Food Additive Regulations 21 CFR 177.1640. The statute and regulations should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Impact Test
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|