Dow CALIBRE® 2060 15 Polycarbonate, Sterilization Grade

 

Subcategory: Polycarbonate; Thermoplastic

Key Words: PC

Material Notes:
CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity when exposed to ethylene oxide. For those applications which use steam sterilization or autoclaving, CALIBRE 2060 series resins offer superior hydrolytic stability for a polycarbonate resin.

Typical applications(1) are hemodialyzers, anesthesia containers, blood oxygenators, arterial filters, intravenous connectors, cardiotomy reservoirs, arteriograph manifolds, blood centrifuge bowls and physiological pressure transducers.

Available Melt Flow Rates: 10, 15.

Associated products:
CALIBRE 2060: without a mold release package
CALIBRE 2061: including a mold release package

(1) NOTICE REGARDING LONG-TERM MEDICAL IMPLANT APPLICATIONS: The Dow Chemical Company does not recommend any medical resin or film product for long-term medical implant applications in humans (more than 72 hours). Further, Dow does nor recommend the use of any medical resin or film product for cardiac prosthetic devices regardless of the time period that the device will be wholly or partially implanted in the body. Such applications include, but are not limited to, pacemaker leads and devices, cardiac prosthetic devices, such as artificial hearts, heart valves, intra-aortic balloon and control systems, and ventricular bypass assist devices. Dow does not recommend any nonmedical grade resin product for use in any human implant applications.

Where available, biocompatibility data relates to resins, not necessarily to fabricated products. Manufacturers of medical devices, equipment and packaging are responsible for determining the suitability of resins for their intended use.

Data provided by Dow Chemical.

Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Izod Impact, Notched
  • Izod Impact, Unnotched
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Tensile Impact Strength
  • Impact Test
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • CTE, linear 20°C
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Oxygen Index
  • Haze
  • Transmission, Visible
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。