Dow CALIBRE® 5051 15 Polycarbonate, 5% Glass Reinforced
Subcategory: Polycarbonate; Thermoplastic; Polymer
Key Words: PC
Material Notes: CALIBRE® 5051 is a 5% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5051 polycarbonate resin exhibits high modulus and excellent dimensional stability. CALIBRE 5051 polycarbonate resin is typically used for in electrical market applications such as electrical boxes, lighting components and electrical connectors. Available Melt Flow Rate: 15. Data provided by Dow Chemical.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Tensile Impact Strength
- Impact Test
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|