Dow CALIBRE® 5101 15 Polycarbonate, 10% Glass Reinforced
Subcategory: Polycarbonate; Thermoplastic; Polymer
Key Words: PC
Material Notes: CALIBRE 5101 is a 10% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5101 resin exhibits high modulus and excellent dimensional stability. CALIBRE 5101 polycarbonate resin is UL listed. CALIBRE 5101 polycarbonate resin is typically used for in electrical market applications such as electrical boxes, lighting components and electrical connectors and in automotive interior applications such as instrument panel retainers. Available Melt Flow Rate: 15. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Charpy Impact Unnotched
- Charpy Impact, Unnotched Low Temp
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|