Dow CALIBRE® IM 401 18 Polycarbonate, Impact Modified
Subcategory: Polycarbonate; Thermoplastic
Key Words: PC
Material Notes: CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM 401 polycarbonate resins exhibit an excellent balance of impact strength and heat resistance. CALIBRE IM401 polycarbonate resins are typically used in applications requiring enhanced impact strength, such as automotive instrument panel components and retainers. Available Melt Flow Rates: 11, 18. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Impact Test
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|