Dow CALIBRE® SF 7070 Polycarbonate, 7% Glass Reinforced Structural Foam Grade
Subcategory: Polycarbonate; Thermoplastic; Polymer
Key Words: PC
Material Notes: CALIBRE® SF7070. is a 7% glass reinforced structural foam ignition resistant polycarbonate resin specially developed for injection molding processing. The CALIBRE 7070 resin provides a high flexural modulus and dimensional stability while maintaining processability and high impact strength. CALIBRE SF7070 is UL listed. CALIBRE SF7070 structural foam resin is typically used for components of transportation equipment, internal machine structures and business machine housings. Available Melt Flow Rate: 15. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|