Dow ISOPLAST® 202LGF40 Polyurethane (PUR-RT), 40% Long Glass Fiber Reinforced
Subcategory: Polyurethane, TP; Thermoplastic; Polymer
Key Words: TPUR
Material Notes: ISOPLAST® 202LGF40 resin is 40% long glass fiber reinforced resin. It offers high modulus and strength, high heat, excellent chemical resistance, and excellent low temperature toughness. Its unique viscosity characteristics allow excellent processing. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Impact Test
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|