Dow MAGNUM® 1040 ABS, Very High impact
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming. The Automotive grades of MAGNUM ABS resins offer a wide range of gloss, viscosity, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 130 to 590 J/m and heat distortion temperatures from 77.C to 90.C are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars and exterior trim parts requiring painting and plating. MAGNUM 1040 ABS resin is often suitable for applications requiring Izod impact strengths of 530 J/m. This low gloss, very high impact grade is one of the more viscous resins having a melt flow rate of about 2.2 g/10 min. and is often used in door sills and glove boxes. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Impact Test
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|