Dow MAGNUM® 555 ABS
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming. The sheet and thermoforming grades of MAGNUM ABS resins provide excellent high and low gloss aesthetics, good thermal color stability, heat and impact resistance and stiffness for uses such as luggage, tool cases, burial vault liners, signs and recreation vehicle applications. Offering ranges in melt flow rates from 1.0 to 4.0, sheet Izod impacts from 130 to 560 J/m and sheet flexural modulus from 1960 to 2070 MPa, MAGNUM ABS resins can fill a variety of needs. MAGNUM 555 ABS resin provides the same flow and gloss as MAGNUM 800 with a slightly higher base resin color and a sheet Izod of 350 J/m. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|