Dow MAGNUM® 9085 ABS

 

Subcategory: ABS Polymer; Thermoplastic

Key Words: Poly(Acrylonitrile Butadiene Styrene)

Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

MAGNUM ABS resins offer a range of gloss and processability options for sprinkler and irrigation applications. Providing high tensile strength with a balance of flow and impact resistance, MAGNUM ABS resins are used in pop-up sprinkler bodies, risers and valves.

MAGNUM 9085 ABS resin is a medium gloss, medium impact, low melt flow rate resin for use in irrigation applications.

Data provided by Dow Chemical.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Melt Flow
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Izod Impact, Notched
  • Flammability, UL94
  • Gloss
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。