Dow MAGNUM® HPC 952 ABS, High Gloss
Subcategory: ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming. The sheet and thermoforming grades of MAGNUM ABS resins provide excellent high and low gloss aesthetics, good thermal color stability, heat and impact resistance and stiffness for uses such as luggage, tool cases, burial vault liners, signs and recreation vehicle applications. Offering ranges in melt flow rates from 1.0 to 4.0, sheet Izod impacts from 130 to 560 J/m and sheet flexural modulus from 1960 to 2070 MPa, MAGNUM ABS resins can fill a variety of needs. MAGNUM HPC 952 ABS resin is the stiffest grade in the high gloss, sheet product line. With a melt flow rate of 1.2 g/10 min., MAGNUM HPC 952 has very good impact strength, good tensile and flexural properties and a Gardner 60. Gloss of 65 - 95 % as measured on thermoformed parts. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Impact Test
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|