Dow PREVAIL® 3100 ABS + Polyurethane
Subcategory: Polyurethane, TP; ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: PREVAIL® 3100 thermoplastic resin offers designers and manufacturers a combination of flexibility and low temperature toughness not previously available in an engineering thermoplastic and is used for applications ranging from flexible bumper fascias to sports equipment components. It is easy to process and is paintable without the need for a primer. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Impact Test
- CTE, linear 20°C
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|