Dow PULSE® 959 ABS + Polycarbonate, 10% Glass Reinforced
Subcategory: Polycarbonate; ABS Polymer; Thermoplastic; Polymer
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: PULSE® 959 Engineering resin is a 10% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 959 Engineering resin has been used in automotive interior trim applications. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Impact Test
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|