Dow RETAIN® 8209 ABS + Polycarbonate
Subcategory: Polycarbonate; ABS Polymer; Thermoplastic
Key Words: Poly(Acrylonitrile Butadiene Styrene)
Material Notes: No text available for this product. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Izod Impact, Notched, Low Temp
- Impact Test
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|