Dow STYRON® 484 High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: HIPS
Material Notes: STYRON® 484 high impact polystyrene resin is typically used in containers, hot and cold drink cups, thin walled packages and other applications. It is an excellent resin for extrusion and thermoforming applications. When used unmodified for the manufacture of food contact articles STYRON 484 complies with the US Food, Drug and Cosmetic Act and Food Additive Regulation 21 CFR 177.1640. The regulation should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|