Dow STYRON® 6187SF High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: PS
Material Notes: STYRON® 6187SF structural foam molding resin is a high impact polystyrene grade with proprietary ignition resistance additive package to achieve UL 94 V-0 rating. It offers excellent moldability and high impact strength. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Vicat Softening Point
- Flammability, UL94
|
|
|
|