Dow STYRON® XL-8023VC High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Key Words: HIPS
Material Notes: STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins. When used unmodified for the manufacture of food contact articles STYRON XL-8023 VC complies with the US Food, Drug and Cosmetic Act and Food Additive Regulations 21 CFR 177.1640. The regulations should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Density
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Izod Impact, Notched
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|