Dow PELLETHANE® 2102-90A Polyurethane Elastomer, Polyester Polycaprolactone Based
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Material Notes: PELLETHANE® 2102-90A elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with low compression set and good hydrolytic stability compared to other polyester based TPUs. Its typical applications include seals, gaskets, belting, animal ID tags and other fabricated products. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 300% Modulus
- Flexural Modulus
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- CTE, linear 20°C
- Vicat Softening Point
- Glass Temperature
- Clash Berg Stiffness Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|