Dow PELLETHANE® 2103-80AEN Polyurethane Elastomer, Ether Based
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Material Notes: PELLETHANE® 2103-80AEN elastomer is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to attack by microorganisms. Its typical applications include film, tubing, belting, and well tank bladders. This resin is listed by National Sanitation Foundation (NSF) (Standard 61). When used unmodified for the manufacture of food contact articles PELLETHANE 2103-80AEN complies with the US Food, Drug and Cosmetic Act and Food Additive Regulations 21 CFR 175.105, 177.2600 and 177.1680. The regulations should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 300% Modulus
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- CTE, linear 20°C
- Vicat Softening Point
- Glass Temperature
- Clash Berg Stiffness Temperature
- Processing Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|