Dow PELLETHANE® 2103-85AE Polyurethane Elastomer, Ether Based
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Material Notes: PELLETHANE® 2103-85AE elastomer is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to attack by microorganisms. Its typical applications include wire and cable jacketing, wheels, film, tubing, and belting. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength at Break
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 300% Modulus
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- CTE, linear 20°C
- Vicat Softening Point
- Glass Temperature
- Clash Berg Stiffness Temperature
- Processing Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|