Dow PELLETHANE® 2355-80AE Polyurethane Elastomer, Polyester Polyadipate Based
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic
Material Notes: PELLETHANE® 2355-80AE elastomer is a polyester polyadipate based polyurethane elastomer which offers 'memory', elasticity, and slightly better oil and chemical resistance than the 2102 series resins. It blends easily with other thermoplastic resins. Data provided by Dow Chemical.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore A
- Tensile Strength at Break
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 300% Modulus
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- CTE, linear 20°C
- Vicat Softening Point
- Glass Temperature
- Clash Berg Stiffness Temperature
- Processing Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|