Dow PELLETHANE® 2363-55D Polyurethane Elastomer, Ether Based

 

Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic

Material Notes:
PELLETHANE® 2363-55D elastomer is a polytetramethylene glycol based polyurethane elastomer used in healthcare applications. Its outstanding properties include superior resilience, low temperature properties, resistance to attack by microorganisms, and excellent hydrolytic stability. It allows sterilization by dry heat, ethylene oxide or gamma radiation. This resin (and other TPUs) should not be sterilized by use of pressurized steam. Its typical applications include catheter components, tensioning ligatures, tubing, connectors and fittings. USP Class VI test data for biocompatibility is available for 2363 series resins.

Data provided by Dow Chemical.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength at Break
  • Elongation at Break
  • 50% Modulus
  • 100% Modulus
  • 300% Modulus
  • Flexural Modulus
  • Tear Strength
  • Taber Abrasion, mg/1000 Cycles
  • Compression Set
  • Compression Set, Elevated Temperature
  • Tensile Set
  • CTE, linear 20°C
  • Vicat Softening Point
  • Clash Berg Stiffness Temperature
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。