Dow PELLETHANE® 2103-90AEFH Film Grade Thermoplastic Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polyurethane, TP; Thermoplastic; Polymer
Material Notes: Description: PELLETHANE® 90AEFH polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications include: Film, Tubing and belting, Geophysical wire and cable jacketing, Cell phones and PDA overmolding Data provided by Dow Chemical.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 300% Modulus
- Flexural Modulus
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- CTE, linear 20°C
- Vicat Softening Point
- Glass Temperature
- Processing Temperature
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|