Dow AFFINITY® HF 1030 Polyolefin Plastomer
Subcategory: Elastomer, TPE; Thermoplastic; Polymer
Material Notes: AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds, and exceptional resistance to draw resonance. It can bring important value to a variety of personal care and medical applications as high performance monolayer films or coextruded films. AFFINITY HF 1030 polymer has excellent compatibility with other polyolefins, allowing efficient blending and coextrusion. AFFINITY HF 1030 polymer complies with FDA regulation 21 CFR 177.1520c3.2a, which allows for its use in direct food contact applications. Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|