Dow AFFINITY® SM 1300 Polyolefin Plastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: AFFINITY® SM 1300 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in high clarity durable injection molded industrial and consumer goods and compression molded closure liners or gaskets. It exhibits excellent optics and flexibility, and allows the use of hot runner molds to enhance production automation. Its low specific gravity can help control resin and production costs, while reducing the weight of end products. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Vicat Softening Point
|
|
|
|
| Property Data |