Dow AFFINITY® SM 8250 Polyolefin Plastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: AFFINITY® SM 8250 polyolefin plastomer is an alpha-olefin resin that offers excellent performance in injection molded clear or colored flexible durable parts. It exhibits excellent clarity and flexibility, excellent low temperature impact properties and allows the use of hot runner molds to enhance production automation. Its low specific gravity can help control resin and production costs, while reducing the weight of end products. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Vicat Softening Point
|
|
|
|
| Property Data |