Dow AFFINITY® VP 8770 Polyolefin Plastomer
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes: AFFINITY® VP 8770 polyolefin plastomer is an alpha-olefin resin for general purpose applications. It exhibits excellent optics and flexibility. Its low specific gravity can help control resin and production costs, while reducing the weight of end products. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
|
|
|
|