Dow ATTANE® 4501 Ultra Low Density Polyethylene, Blown Film Grade
Subcategory: Polyethylene; Thermoplastic; LDPE; Polymer
Key Words: ULDPE, VLDPE
Material Notes: ATTANE® 4501 copolymer is an ultra low density polyethylene having high tear strength and impact resistance, designed for use in industrial/ consumer film applications, either as a high performance monolayer blown film or as part of a multilayer film. It has low levels of slip and antiblock additives. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2a for food contact. Film properties below based on a film thickness of 38 µm. Data provided by Dow Chemical.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Coefficient of Friction
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|