Dow DOWLEX® 2045.02AC Linear Low Density Polyethylene, Blown Film Grade
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medium level of antiblock additive. It complies with U.S. FDA regulation 21 CFR 177.1520 (c) 3.2 (a) for food contact applications, and has been approved by USDA for packaging meat and poultry products. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Coefficient of Friction
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop Test
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|