Dow DOWLEX® 2056A Linear Low Density Polyethylene, Heavy Duty Film Grade
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: DOWLEX® 2056A Polyethylene is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer with improved thermal stability and is an outstanding choice for critical film applications. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 when used unmodified and according to good manufacturing practices for food contact applications, including packing or holding food during cooking. The regulation should be consulted for complete details. Film properties below based on a film thickness of 30 µm. Data provided by Dow Chemical.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Tensile Strength, Ultimate
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|