Dow DOWLEX® 2071 Linear Low Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: DOWLEX® 2071 Polyethylene resin is a linear low density polyethylene resin specifically designed for the manufacture of high strength, thin gauge films for use in applications such as grocery sacks and trash bags. It contains high level of slip additive and medium level of antiblock additive. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.1 (a) for food packaging applications. The regulation should be consulted for complete details. Film properties below based on a film thickness of 38 µm. Data provided by Dow Chemical.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Coefficient of Friction
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|