Dow DOWLEX® 2245D Linear Low Density Polyethylene, Heavy Duty Film Grade
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes: DOWLEX® 2245D Polyethylene resin is a premier film resin for heavy duty applications. DOWLEX 2245D resin is used where improved thermal stability over a broad range of processing conditions is necessary. This material complies with U.S. FDA Regulation 21 CFR 177.1520 c 3.2(a) food packaging applications. The regulation should be consulted for complete details. Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Tensile Strength, Ultimate
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Strength, Yield
- Elongation at Break
- Secant Modulus, MD
- Secant Modulus, TD
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Vicat Softening Point
- Haze
- Gloss
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|