Dow DOWLEX® 2535 Linear Low Density Polyethylene, Narrow MW Distribution
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: DOWLEX® 2535 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and stress crack resistance with good flexibility. It has good processability over a wide range of molding conditions. This material complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.1 (a) for food packaging applications. The regulation should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact, Notched, Low Temp (ISO)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|