Dow DOWLEX® IP-10 High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Next Generation DOWLEX® IP-10 resin is a high density polyethylene resin specifically designed for reusable case applications including, poultry, fast food, automotive, retail, fresh produce, beverage (soft drinks), food service and chemicals, including plastics. Excellent processability is achieved with Next Generation DOWLEX IP-10 resin due to its easy flow at low temperatures. This material complies with FDA regulation 21 CFR 177.1520 c 3.2 (a) for food contact applications. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact Resistance
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|