Dow DOWLEX® IP-22 High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: DOWLEX® IP-22 resin is an improved processing high density polyethylene resin designed for excellent flow, high impact, and moderate stiffness. DOWLEX IP-22 resin balances peak molecular weight with a proprietary, optimized molecular weight distribution and a slightly lower density for impact and integrity. Typical applications are housewares, toys and general purpose applications. This material complies with FDA regulation 21 CFR 177.1520 c 3.1 for food contact applications. The regulation should be consulted for complete details. Data provided by Dow Chemical.
| Available Properties |
- Density
- Viscosity
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact Resistance
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|