Dow DOWLEX® IP-41 High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: DOWLEX® IP-41 resin is an improved processing high density polyethylene resin designed to offer excellent processability and rigidity required for food containers, overcaps, and other general purpose applications. DOWLEX IP-41 resin balances peak molecular weight with a proprietary, optimized molecular weight distribution and a slightly higher density for excellent rigidity. This resin has demonstrated excellent processability over a wide range of molding conditions. This material complies with FDA regulation 21 CFR 177.1520 (c) 3.2 (a) for food contact applications. Data provided by Dow Chemical.
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Izod Impact Resistance
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|